Description: ASTM A131 Grade D marine steel plates belong to general strength shipbuilding steel. The equivalent grades of ASTM A131 grade D steel are ABS D, BV D, CCS D, NV D, GL-D, RD, LR D, KD, RINA D, etc. ASTM A131 Grade D shipbuilding steel plates contain chemic...
If the standard size steel materials can not meet your demands, We aslo supply ASTM A131 Grade D steel processing service. you can find one-stop solution for various customized steel processing requirements: Large vessels, structural parts, semi-products, components, manufacturing supporting ...
Processing Service: Cutting, Welding, Drilling, Rolling, Bending, Forming, Grinding, Stamping and so on machining
ASTM A131 Grade D marine steel plates belong to general strength shipbuilding steel. The equivalent grades of ASTM A131 grade D steel are ABS D, BV D, CCS D, NV D, GL-D, RD, LR D, KD, RINA D, etc. ASTM A131 Grade D shipbuilding steel plates contain chemical elements that resist corrosion and decrease brittleness, especially in cold temperatures, and increase strength and toughness to resist vibration and force traumas.
ASTM A131 Grade D shipbuilding steel plates are used in the ship project and ocean offshore structural project, for making the offshore oil drilling platform, the hull of ship building and ship repairing, the platform pipe joints and other components. ASTM A131 Grade D hull steel plate shall do charpy V-notch test when the thickness is above 1/4 in. [6.4mm].
Thickness: 3mm-150mm
Width: 1220 - 4220mm
Length: 5000-18000mm
Standard: ASTM A131
Classification Societies: ABS, LR, BV, DNV GL, RINA, NK, CCS, KR, RMRS
Surface Treatment: Clean, blasting and painting according to customer requirement
Export packing: Waterproof paper, and steel strip packed.
Standard Export Seaworthy Package.Suit for all kinds of transport,or as request
Capacity: 250,000 tons/year
(heat analysis, % max unless otherwise specified)
C | Mn | Si | P | S | C+Mn/6 |
---|---|---|---|---|---|
0.21 | 0.6 | 0.10-0.35 | 0.035 | 0.035 | 0.40 |
Notes: The contents of nickel, chromium, molybdenum, and copper are to be determined and reported. When the amount does not exceed 0.02 %, these elements may be reported as≤0.02 % .
Crack Sensitivity: Pcm = (C+Si/30+Mn/20+Cu/20+Ni/60+Cr/20+Mo/15+V/10+5B)%
Carbon Equivalent: Ceq = 【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
Grade |
Mechanical Property | Charpy V Impact Test | ||||
---|---|---|---|---|---|---|
Thickness | Yield | Tensile | Temperature | Transverse | Longitudinal | |
ASTM A131 grade D | mm | Min Mpa | Mpa | 20℃ | J | J |
t≤50 | 235 | 400-520 | 20 | 27 | ||
50<t≤70 | 235 | 400-520 | 24 | 34 | ||
70<t≤100 | 235 | 400-520 | 27 | 41 |
Notes: Impact tests are not required when the material is produced using fine grain practice and normalized.
ABS | LR | BV | DNV | GL | RINA | NK | CCS | KR | RMRS |
---|---|---|---|---|---|---|---|---|---|
ABS D | LR D | BV D | NV D | GL D | RINA D | KD | CCS D | RD | RMRS D |